Mechanical and Electrical Properties of Heat-Treated Ladder Polymer Fiber

The ladder polymer poly was synthesized in polyphosphoric acid at a concentration of 15% by weight

C. S. Wang; C. Y-C Lee; F. E. Arnold

2011

Scholarcy highlights

  • The ladder polymer poly was synthesized in polyphosphoric acid at a concentration of 15% by weight
  • The fiber exhibited a phosphoms content below the detectable limit by elemental analysis
  • After neutralization, the fiber exhibited a phosphoms content below the detectable limit by elemental analysis